(High Elastic Protective and Waterproofing Slurry) A cement base, 2 component polymer modified high elastic waterproofing slurry. It is applied to concrete and mortar structures to prevent water infiltration.
A cement base, 2 component polymer modified high elastic waterproofing slurry. It is applied to concrete and mortar structures to prevent water infiltration.
Due to its high elasticity, Rock Seal 777 (Elastic is applicable on different structures including those subject to thermal movement and vibration as: Waterproofing and protection of structures under hydraulic pressure, like water storage tanks, swimming pools, concrete pipes, bridge parapets, water canals, sewage treatment structures….etc.
Waterproofing and protection of external walls to be buried below ground.
Internal waterproofing against hydrostatic water pressure of walls and floors in basements and other below ground structures.
Waterproofing of terraces and balconies on concrete and old tiles substrates.
Protection of exposed and weathered, new and existing concrete surfaces, as anti-carbonation and as cover compensating in case of insufficient
cover (2 mm Rock Seal 777 (Elastic) is equivalent to 6 inches of concrete)
Elastic coating of precast concrete surfaces, subject to flexural loading and vibration, etc
Rock Seal 777 (Elastic) shall be mixed with a low speed (< 500 rpm) electric drill mixer. Pour the liquid component (A) into a suitable mixing container. While stirring slowly, add the powder component (B) to component A. Mix thoroughly for at least 3 minutes to the required consistency.
While the surface is still damp (no standing water)
apply the first coat and leave to harden
(2-6 hours). For slurry consistency, apply with a hard-plastic bristled brush or broom. For trowelable mortars, use a notched trowel. After the second coat has been applied, finish by rubbing down with a soft dry sponge.
Minimum ambient and substrate temperature+8
In severe heat and/or wind, protection of the Rock Seal 777 (Elastic) is recommended. As with all cement based products, curing is important. Protect newly applied product against direct sunlight, wind, rain and frost
DISCRIPTION |
VALUE |
Colour |
Grey |
Chemical Base |
Part A: liquid (Styrene acrylic) polymer and additive Part B: Portland cement selected aggregate and admixtures |
Density |
Comp (A+B) = 1.7 kg/I (mixed) |
Compressive Strength |
30 - 40 N/mm2 at 20°C after 28 days (mortar consistency) |
Flexural Strength |
10 - 12 N/mm2 at 20°C after 28 days (mortar consistency) |
Bond Strength |
Approx. 1 N/mm2 after 28 days (sand blasted) |
Mixing Ratio |
Slurry 1: 2 by weight |
Initial Tensile adhesion strength |
> 0.5 N/mm2 |
Crack Bridging ability at 23 C |
> 1.0 mm. |
Tensile adhesion 28d after water immersion |
> 0.5 N/mm2 |
Elongation at break |
120 – 140% |
Do not dispose of into water or soil, but according
to local regulations.
Non-hazardous.
Wear gloves and goggles. In contact with eyes or skin product, may cause irritation.
Non-Toxic under relevant health and safety codes.
Concrete, mortar and masonry surfaces must be clean, free from grease, oil and loosely adhering particles. All surfaces must be as true and flat as possible. Saturate absorbent surfaces thoroughly with water before application.
Depending on type of application, two (2) coats always required. Three (3) coats may be required in areas of extremely high infiltration. 1st coat consumption 1-1.5 kg/m2 on damp surface.
2nd coat consumption 0.8 - 1 kg/m2 approx.