ROCKAL Rock wool Boards are composed of mineral rock fibers, processed from volcanic basaltic rocks, Fibers are bonded together with a thermosetting binder which gives the flexibility & resilience to the product.
Rock wool board insulation is a type of rigid insulation made from spun mineral wool, which is derived from a mixture of volcanic rock and slag.
It is known for its high thermal resistance, soundproofing capabilities, and fire-resistant properties, making it a popular choice for insulation in a wide range of applications.
ROCKAL Boards are especially rigid than other ROCKAL Rock wool products and comply with ASTM C-612.
ROCKAL Rock wool Boards can be non-Faced or faced with reflective vapor barrier material (Reinforced Aluminum Foil FSK) or Kraft Paper, fiber glass tissue BGT or BGF.
ROCKAL Rock wool fibers products are classified as Non-Combustible materials and follow the fire safety rating achievements:
In summary, rock wool board insulation is a versatile and durable insulation solution that offers excellent fire resistance, soundproofing properties, and resistance to moisture and mold. It is an energy-efficient and environmentally friendly option for a wide range of insulation applications.
Property | Value | |
Service Temp. (Hot Side) | 400°C to 750 C | |
Melting Temp. | 1500°C | |
Outer Facing Temp. Range | -29°C to 66°C | |
Moisture Absorption |
< 1% (By weight, Water repellant, Non-Hygroscopic, Non-Capillary
No Effect on Stability |
|
Corrosion Resistance | PH 7 or Slightly Alkaline | |
Soluble Chlorides | 6 PPM | |
Fungi Resistance | Doesn’t encourage Fungi growth | |
Noise Reduction Coefficient (NRC) |
≈ 0.85 |
|
Asbestos Content | Non-Toxic and not hazardous to health and Asbestos Free
Does not contain: AMPHIBOLE {CA2 MG3(OH)2 SI8 O22} Nor SERPENTINE Asbestos {MG3 SI2 (OH)4 O5} |
|
Environment | CFC and HCFC Free | |
Expansion and Contraction | Completely Stable | |
Shot Content | Less than 25% | ASTM C-1335 |
Condensation | The vapor diffusion of Rockal Rock wool is negligible it’s considered
zero compared to other insulation materials |
|
Rigidity | Rigid | ASTM C-1101 / M |
Thermal Conductivity For the following densities in(Kg/M3) |
||||||||
Mean Temperature (°C) | 35 | 40 | 50 | 70 | 100 | 128 | 140 | |
10 | 0.036 | 0.036 | 0.036 | 0.038 | 0.037 | 0.038 | 0.038 | |
50 | 0.036 | 0.036 | 0.036 | 0.038 | 0.037 | 0.039 | 0.035 | |
100 | 0.046 | 0.047 | 0.047 | 0.046 | 0.046 | 0.049 | 0.039 | |
150 | 0.054 | 0.054 | 0.055 | 0.053 | 0.054 | 0.053 | 0.041 | |
200 | 0.066 | 0.067 | 0.068 | 0.064 | 0.060 | 0.058 | 0.049 | |
250 | 0.081 | 0.082 | 0.084 | 0.080 | 0.081 | 0.069 | 0.056 | |
350 | 0.112 | 0.122 | 0.124 | 0.120 | 0.121 | 0.091 | 0.084 | |
450 | 0.131 | 0.142 | 0.146 | 0.135 | 0.136 | 0.139 | 0.132 |